TAPPI T 569 om-14
Click here to purchase
This method defines a test that measures the energy required to rapidly delaminate a sheet-type speciment. The “Z” directional rupture is initiated by the impact of a pendulum having both a controlled mass and a controlled velocity that exceeds 6000 times the velocity of tensile strength and other dead-weight testers. The geometry of the apparatus causes the tensile stress to be rotational in nature with negligible shear stress on the specimen.
The method is suitable for both single and multi-ply paper and paperboard, including coated sheets and those that are laminated with synthetic polymer films.
Product Details
- Published:
- 2014
- ANSI:
- ANSI Approved
- Number of Pages:
- 9
- File Size:
- 1 file , 86 KB
- Redline File Size:
- 2 files , 2.9 MB