AASHTO R 78-22

Click here to purchase

This practice covers two methods for recovering the residue from emulsified asphalts such as those specified in AASHTO M 140 and M 208, using low-temperature evaporative techniques that are similar to pavement conditions. The recovered residue can be used for further testing as required.

This standard was formerly designated as provisional standard PP 72.